Comparison

Carbon Fiber PPS vs PEEK

A side-by-side comparison of Polyphenylene Sulfide, Carbon Fiber Reinforced and Polyether Ether Ketone.

Physical

Density
1.55-1.70 g/cm³
1.32 g/cm³
Water Absorption (24h)
0.01-0.05 %
0.15 %
Transparency
Opaque
Opaque (amber)
Shrinkage
0.1-0.3 %
1.1 – 1.4 %

Mechanical

Young's Modulus
18-25 GPa
3.6 GPa
Tensile Strength
120-150 MPa
100 MPa
Elongation at Break
1-3 %
50 %
Impact Strength (Izod)
5-10 kJ/m
55 J/m
Flexural Strength
170 MPa

Thermal

Glass Transition Temperature
100-120 °C
143 °C
Melting Point
275-285 °C
343 °C
Continuous Service Temperature
200-240 °C
260 °C
Heat Deflection Temperature
260-280 °C (1.8 MPa)
160 °C

Electrical

Dielectric Constant
N/A (conductive)
3.2
Volume Resistivity
10^2-10^5 Ohm-cm
10¹⁶ Ω·cm
Dielectric Strength
Low (conductive)

Chemical resistance

Acids
Excellent
Excellent
Bases
Excellent
Excellent
Solvents
Excellent
Excellent
UV Resistance
Good
Fair
Hydrolysis (steam)
Excellent

Sustainability

Recyclability
Recyclable (difficult)
Recyclable (specialty)
Recycling Code
7 (Other)
7
Carbon Footprint
High
~30 kg CO₂e / kg