Physical
Density
1.32 g/cm³
1.04 – 1.07 g/cm³
Water Absorption (24h)
0.15 %
0.20 – 0.45 %
Transparency
Opaque (amber)
Opaque
Shrinkage
1.1 – 1.4 %
0.4 – 0.9 %
Specific Gravity
—
1.05
Surface Finish
—
Matte to glossy
Mechanical
Young's Modulus
3.6 GPa
1.8 – 2.5 GPa
Tensile Strength
100 MPa
40 – 50 MPa
Flexural Strength
170 MPa
60 – 80 MPa
Impact Strength (Izod)
55 J/m
200 – 400 J/m
Elongation at Break
50 %
10 – 50 %
Hardness (Rockwell R)
—
100 – 115
Thermal
Melting Point
343 °C
Amorphous (no true Tm)
Glass Transition Temperature
143 °C
105 °C
Continuous Service Temperature
260 °C
70 – 90 °C
Heat Deflection Temperature
160 °C
85 – 100 °C
Thermal Conductivity
—
0.17 W/m·K
CTE
—
80 – 100 × 10⁻⁶ /K
Electrical
Dielectric Constant
3.2
2.7 – 3.2
Volume Resistivity
10¹⁶ Ω·cm
10¹⁶ Ω·cm
Surface Resistivity
—
10¹⁵ Ω
Dielectric Strength
—
15 – 20 kV/mm
Chemical resistance
Acids
Excellent
—
Bases
Excellent
Good
Solvents
Excellent
—
Hydrolysis (steam)
Excellent
—
UV Resistance
Fair
Poor (unless stabilized)
Acids (dilute)
—
Good
Alcohols
—
Good
Oils & Greases
—
Fair
Gasoline
—
Poor
Acetone
—
Attacks / dissolves
Weathering
—
Poor without stabilizers
Sustainability
Recyclability
Recyclable (specialty)
Recyclable (mechanical)
Recycling Code
7
7 (Other)
Carbon Footprint
~30 kg CO₂e / kg
~3.1 kg CO₂e / kg
Bio-based Content
—
0 %