Comparison

PHA Flexible Grade D vs PEEK

A side-by-side comparison of Polyhydroxyalkanoate, Flexible Grade D and Polyether Ether Ketone.

Physical

Density
1.20 g/cm³
1.32 g/cm³
Water Absorption (24h)
0.8 %
0.15 %
Transparency
Moderate
Opaque (amber)
Shrinkage
2.0 - 4.5 %
1.1 – 1.4 %

Mechanical

Young's Modulus
0.5 GPa
3.6 GPa
Tensile Strength
30 MPa
100 MPa
Elongation at Break
15.0 %
50 %
Impact Strength (Izod)
1.0 J/cm
55 J/m
Flexural Strength
170 MPa

Thermal

Glass Transition Temperature
-5 °C
143 °C
Melting Point
110-120 °C
343 °C
Continuous Service Temperature
40 °C
260 °C
Heat Deflection Temperature
35 °C
160 °C

Electrical

Dielectric Constant
3.0
3.2
Volume Resistivity
10¹¹ Ω·cm
10¹⁶ Ω·cm
Dielectric Strength
15 kV/mm

Chemical resistance

Acids
Good resistance
Excellent
Bases
Good resistance
Excellent
Solvents
Resistant to aliphatic hydrocarbons, but attacked by chlorinated and aromatic hydrocarbons
Excellent
UV Resistance
Moderate
Fair
Hydrolysis (steam)
Excellent

Sustainability

Recyclability
Biodegradable (soil, marine, compost)
Recyclable (specialty)
Recycling Code
7 (Other)
7
Carbon Footprint
Low
~30 kg CO₂e / kg