Physical
Density
1.10-1.30 g/cm³
1.04 – 1.07 g/cm³
Water Absorption (24h)
0.5-1.5 %
0.20 – 0.45 %
Transparency
Opaque (typically black)
Opaque
Shrinkage
0.5-1.5 %
0.4 – 0.9 %
Specific Gravity
—
1.05
Surface Finish
—
Matte to glossy
Mechanical
Young's Modulus
0.02-0.10 GPa
1.8 – 2.5 GPa
Tensile Strength
30-60 MPa
40 – 50 MPa
Elongation at Break
300-600 %
10 – 50 %
Impact Strength (Izod)
N/A (flexible grade)
200 – 400 J/m
Flexural Strength
—
60 – 80 MPa
Hardness (Rockwell R)
—
100 – 115
Thermal
Glass Transition Temperature
-30 to -10 °C
105 °C
Melting Point
N/A (elastomeric)
Amorphous (no true Tm)
Continuous Service Temperature
70-90 °C
70 – 90 °C
Heat Deflection Temperature
N/A
85 – 100 °C
Thermal Conductivity
—
0.17 W/m·K
CTE
—
80 – 100 × 10⁻⁶ /K
Electrical
Dielectric Constant
4.0-5.0
2.7 – 3.2
Volume Resistivity
10^10-10^12 Ohm·cm
10¹⁶ Ω·cm
Dielectric Strength
10-20 kV/mm
15 – 20 kV/mm
Surface Resistivity
—
10¹⁵ Ω
Chemical resistance
Acids
Good resistance
—
Bases
Good resistance
Good
Solvents
Resistance varies, attacked by strong polar solvents
—
UV Resistance
Fair (can degrade over time)
Poor (unless stabilized)
Acids (dilute)
—
Good
Alcohols
—
Good
Oils & Greases
—
Fair
Gasoline
—
Poor
Acetone
—
Attacks / dissolves
Weathering
—
Poor without stabilizers
Sustainability
Recyclability
Recyclable (check local facilities)
Recyclable (mechanical)
Recycling Code
7 (Other)
7 (Other)
Carbon Footprint
Lower than virgin TPU
~3.1 kg CO₂e / kg
Bio-based Content
—