Comparison

Tough Abrasion-Resistant Thermoplastic Polyurethane (Polyester) vs PA66

A side-by-side comparison of Thermoplastic Polyurethane (TPU) - Polyester type and Polyamide 6,6 (Nylon).

Physical

Density
1.14 - 1.25 g/cm³
1.14 g/cm³
Water Absorption (24h)
0.5 - 1.5 %
1.2 %
Transparency
Opaque to Translucent
Opaque
Shrinkage
0.5 - 1.5 %
1.5 – 2.0 %

Mechanical

Young's Modulus
0.02 - 0.2 GPa
3.0 GPa (dry)
Tensile Strength
20 - 60 MPa
80 MPa
Elongation at Break
400 - 700 %
60 %
Impact Strength (Izod)
High (10-100+ J/m, notched)
50 J/m
Flexural Strength
110 MPa

Thermal

Glass Transition Temperature
-10 to 10 °C
70 °C
Melting Point
150 - 200 °C
255 – 265 °C
Continuous Service Temperature
-30 to 80 °C
100 – 120 °C
Heat Deflection Temperature
40 - 70 °C
75 °C (unfilled)

Electrical

Dielectric Constant
5.0 - 6.0
4.0
Volume Resistivity
10^10 - 10^12 Ohm-cm
10¹² Ω·cm
Dielectric Strength
15 - 25 kV/mm

Chemical resistance

Acids
Good
Poor
Bases
Good
Good
Solvents
Good resistance to oils, greases; swells in strong acids, ketones, and certain solvents
UV Resistance
Fair to Good (can yellow)
Fair
Alcohols
Good
Oils & Fuels
Excellent

Sustainability

Recyclability
Recyclable (thermoplastic)
Recyclable
Recycling Code
7 (Other)
7
Carbon Footprint
Moderate
~7.4 kg CO₂e / kg
Bio-based Content
0 – 100 % (bio grades)