Arkema · Grade
RILSAMID AMNO TLD
PA12
This natural grade is designed for injection molding.
Manufacturer
Arkema
Status
active
Technical properties
| Melt volume flow rate, MVR (235°C/2.16kg) | 57 cm³/10min |
| Shrinkage, parallel | 1.2 % |
| Shrinkage, normal | 1.4 % |
| Tensile modulus (23°C) | 1450 MPa |
| Yield strain (23°C) | 7 % |
| Yield stress (23°C) | 42 MPa |
| Nominal strain at break (23°C) | >50 % |
| Charpy notched impact strength, 23°C | 9 kJ/m2 |
| Charpy notched impact strength, -30°C | 5 kJ/m2 |
| Stress at break (23°C) | 64 MPa |
| Vicat softening temperature (50N, 50°C/h) | 142 ℃ |
| Heat deflection temperature (0.45MPa) | 135 ℃ |
| Heat deflection temperature (1.8MPa) | 55 ℃ |
| Melting temperature (10°C/min) | 178 ℃ |
| Burning behavior (1.5mm thickness) | HB |
| Burning behavior (3.0mm thickness) | V-2 |
| Surface resistivity (23°C) | 1.0E+14 ohm/sq |
| Volumic transversal resistivity (23°C) | 1.0E+12 ohm.m |
| Comparative tracking index (23°C) | 600 |
| Relative permittivity (100Hz) | 4 |
| Relative permittivity (1Mhz) | 3 |
| Dissipation factor (100Hz) | 779 E-4 |
| Dissipation factor (1Mhz) | 290 E-4 |
| Dielectric Strength (23°C) | 30 kV/mm |
| Water absorption, at equilibrium (23°C/50%RH) | 0.7 % |
| Density (23°C) | 1.02 g/cm3 |
| Water absorption, at equilibrium (23°C/Immersion) | 1.8 % |
Indicative values. Always consult the manufacturer's official datasheet before specification.
RILSAMID AMNO TLD equivalents
No verified equivalents indexed yet.
Manufacturer
Arkema
Browse all indexed grades